TiN [Titanium Nitride]

Microhardness:
2300HV0.05
Coefficient of Friction:
0.4
Max. Service Temp:
1112 °F / 600 °C

AlCrN [Aluminum Chromium Nitride]

Microhardness:
3200HV0.05
Coefficient of Friction:
0.35
Max. Service Temp:
2012 °F / 1100 °C

TiCN [Titanium Carbo-Nitride]

Microhardness:
3000HV0.05
Coefficient of Friction:
0.4
Max. Service Temp:
752 °F / 400 °C

WC/C [Tungsten Carbide/Carbon]

Microhardness:
1500HV0.05 / 1000HV0.05
Coefficient of Friction:
0.1–0.2
Max. Service Temp:
572 °F / 300 °C

CrN [Chromium Nitride]

Microhardness:
1750HV0.05
Coefficient of Friction:
0.5
Max. Service Temp:
1292 °F / 700 °C

DLC [Diamond-Like Carbon]

Microhardness:
>2000HV0.05
Coefficient of Friction:
0.1–0.2
Max. Service Temp:
662 °F / 350 °C

TiAlN [Titanium Aluminum Nitride]

Microhardness:
3300HV0.05
Coefficient of Friction:
0.3–0.35
Max. Service Temp:
1652 °F / 900 °C

TiAlNx [Titanium Aluminum Nitride]

Microhardness:
3400HV0.05
Coefficient of Friction:
0.3–0.35
Max. Service Temp:
1652 °F / 900 °C